Leave Your Message

What should be noted when processing special-shaped copper bars?

2026-03-19

What should be noted when processing special-shaped copper bars?


1. Material selection and pre-treatment
Material selection: Prefer T2, TU1 oxygen-free copper to ensure high conductivity (≥98% IACS) and ductility; for high current/high heat dissipation scenarios, copper alloys (such as chromium-zinc copper) can be selected.
Inspection of raw materials: Confirm no cracks, inclusions, severe oxidation; thickness / width deviation should comply with standards (≤±0.15~0.3mm).
Surface treatment: Heat-rolled blanks undergo acid washing to remove oxide layer, cold-rolled blanks are scraped or ground to remove oil stains and oxide layer.
Strain relief: Before bending / cold processing, anneal at 350–400℃ for 2 hours to eliminate internal stress and prevent cracking.

2. Core processing techniques

  • Cutting / material cutting
    First laser / CNC cutting to ensure vertical cuts without burrs; length error ≤±1mm.
    Avoid repeated cutting to prevent edge hardening and subsequent bending cracking.
  •  Bending (the most prone to problems)
    Minimum bending radius: flat bending ≥ 2 times thickness; vertical bending ≥ 3 times thickness; when twisting 90°, twisting length ≥ 2.5–5 times width.
  • Mold matching: R angle and thickness correspond (8mm uses R8, 10mm uses R10); special vertical bending / slot-shaped molds are used for special shapes.
  • Operation control: Symmetrical positioning, slow speed (2–5mm/s); do not reverse bend at the original bending point; ensure consistent bending degree for multiple sheets.
  • Quality requirements: Angle error ≤±0.5°; no cracks, wrinkles, flattening.

copper busbar 1.png

3. Punching / drilling

Punch diameter is 0.5–1mm larger than the bolt; hole position error ≤0.5mm; hole is vertical and not skewed.
Use tap drill (depth ≤0.8mm) instead of coarse file; contact surface is pressed and leveled to adjust flatness, with section loss ≤3%.
4. Forming (extrusion / rolling / forging)
Extrusion: Preheat T2 copper at 450–500℃, speed 5–15m/min, lubricate with graphite + molybdenum disulfide.
Rolling: Rollers have precision IT6 grade, tension control ±1%, prevent section distortion.
Forging: For closed structures, use precision forging, key dimensions have tolerance of ±0.02mm.

5 Precision and size control
Section size: ≤10mm ±0.15mm; 10–30mm ±0.2mm; >30mm ±0.3mm.
Straightness: ≤0.5mm/m; flatness ≤0.2mm/m.
Surface roughness: Ra ≤1.6μm (conductive contact surface Ra ≤0.8μm).

6. Surface and post-processing
Cleaning: After processing, thoroughly remove oil stains and copper chips to prevent increased contact resistance.
Protection: Conductive contact surfaces are plated with tin (≥5μm) or silver; insulation parts are coated with plastic / sprayed.
Marking: Clearly label specifications, materials, and batches for easy traceability.
7. Quality inspection
Full inspection: dimensions, angles, straightness, surface defects.
Sampling inspection: conductivity, hardness, coating thickness, non-destructive bending testing.