Production Process of Copper Foil Flexible Connectors
As a core flexible conductor for high-current applications such as new energy energy storage, power transmission and distribution, and rail transit, the quality of copper foil flexible connectors is largely determined by manufacturing procedures. Xi'an Zipeng Technology has years of experience in the manufacturing and foreign trade of copper foil flexible connectors. Below is a systematic introduction to the mainstream production process adopting polymer diffusion welding for our customers and industry peers.
A copper foil flexible connector is stacked from multiple layers of high-purity T2 copper foil. Both ends are welded and consolidated while the middle section remains flexible and bendable. The reliability of a copper foil flexible connector mainly depends on whether the terminals are fully and firmly welded. There are two mainstream technical routes in the industry: polymer diffusion welding (solder-free metallurgical bonding) and brazing. Xi'an Zipeng Technology fully adopts the polymer diffusion welding process and implements production under the IATF16949 automotive quality management system. The complete production flow is shown as follows.
Step 1: Uncoiling, slitting and cutting. T2 electrolytic copper foil coils (common thickness: 0.05 mm, 0.1 mm, 0.2 mm) are slit to the required width according to drawings and then cut to specified lengths. The stacking layer count is calculated precisely based on the target cross-sectional area to meet the current-carrying requirement of the copper foil flexible connector.
Step 2: Cleaning, degreasing and deoxidation. Oil stains, fingerprints or oxide layers on copper foil surfaces will directly cause poor welding and delamination after diffusion welding. Xi'an Zipeng Technology combines ultrasonic cleaning and pickling passivation, followed by thorough drying to guarantee clean bonding surfaces. This procedure is critical to ensure terminal strength of copper foil flexible connectors.
Step 3: Stack alignment and fixture positioning. Copper foils are neatly stacked by required layers. The welding zones on both ends are precisely aligned while the flexible middle part stays loose, then fixed by custom jigs. The fixture ensures uniform pressure and prevents misalignment or warping.
Step 4: Polymer diffusion welding (core process). Only the two end terminals of the copper foil flexible connector are welded; the middle flexible segment remains unwelded. Under the conditions of 500–620 ℃, pressure of 10–30 MPa and holding time, copper atoms interpenetrate to form solder-free solid-state metallurgical bonding. Multiple copper foil layers are integrated into a solid copper block. Slow cooling under pressure after welding releases internal stress to avoid microcracks and springback deformation. Compared with brazing, connectors made by diffusion welding feature terminal resistance close to base copper, excellent vibration resistance and stable performance under thermal cycling, making them the preferred choice for new energy and power projects.
Step 5: Deburring and grinding. Weld beads and burrs on the front, back and side surfaces of terminals are polished to smooth edges, preventing insulation piercing in subsequent processes.
Step 6: Machining, drilling and counterboring. Holes and counterbores are machined according to customer bolt specifications. Counterbore ensures full contact of bolt surfaces and stable contact resistance.
Step 7: Surface plating (optional). Tin plating is widely used for distribution cabinets and BMS for oxidation resistance. Nickel plating is selected for scenarios requiring high temperature resistance and salt spray resistance. Silver plating is applied for 800 V high-voltage platforms and high-power modules to achieve minimum contact resistance. Partial or full plating is available.
Step 8: Insulation cladding (optional, mandatory for high voltage). Protection methods include heat shrink tubing, fiberglass sleeve, Mylar film coating and epoxy potting to guarantee safe operation under high voltage.
Step 9: Bending and forming. Bending is carried out per drawings with controlled minimum bending radius. Sharp dead folding is forbidden to avoid copper foil fatigue fracture.
Step 10: Full inspection and performance test. Tests cover appearance check, dimension measurement, DC resistance test, tensile test, voltage withstand test, salt spray test, thermal cycling test and sampling temperature rise test to guarantee every delivered copper foil flexible connector is qualified.
Step 11: Marking, packaging and warehousing. Labels with model, current rating and batch number are attached. Anti-static packaging is adopted to prevent oxidation and damage during transportation.
Xi'an Zipeng Technology believes that the value of copper foil flexible connectors lies in long-term reliability rather than mere appearance. Every working procedure affects temperature rise and operational safety under live conditions. We stick to diffusion welding and full-process quality inspection, so our copper foil flexible connectors can serve stably in energy storage cabinets, traction converters and rectifier cabinets.
Need a sample for testing? welcome to mail: info@zpbusbar.com