Copper Foil Flexible Connector Welding Solution
Copper Foil Flexible Connector Welding Solution
Xi'an Zipeng Technology Xi'an Zipeng Technology specializes in R&D and export manufacturing of laminated copper foil flexible connectors. Serving overseas projects including transformers, energy storage systems and BMS sensing devices, we adopt solid-state diffusion welding as the core welding process for flexible copper connectors. This solder-free process realizes metallurgical bonding between copper foil atoms under high temperature and high pressure. We strictly separate rigid welded zones and flexible sliding zones, ensuring integrated solid terminals while retaining slidable multi-layer copper foil in the middle flexible section. The product meets long-term anti-vibration and temperature-cycle operation requirements for Middle East, European and American foreign trade projects.
1. Pre-welding Preparation
Surface cleaning before welding is fundamental to eliminating cold joints and delamination defects. C11000 annealed soft copper foil is adopted and cut by CNC equipment to guarantee burr-free edges. Ultrasonic alkaline cleaning and mild acid micro-etching are applied to remove oil, fingerprints and oxide film on copper foil surfaces, followed by three-stage deionized water rinsing and hot-air drying to fully eliminate surface contaminants. Multiple copper foils are neatly stacked and positioned with tooling, and the layer misalignment is controlled within 0.2 mm. Only the two terminal zones enter the welding station; the middle flexible section remains uncompressed. No spot welding or bonding is allowed in flexible zones to prevent loss of elasticity. After stacking, pre-compression and degassing are performed gradually to expel air between layers and avoid pores and voids after welding.
2. Core Diffusion Welding Process
Special rectangular flat dies are used. The die width fully matches the busbar width, and the welding boundary forms a straight line perpendicular to the conductor axis. The process parameters are set according to copper foil layers and total thickness: temperature 500~620℃, pressure 10~30 MPa, holding time 10~60 seconds. Under constant temperature and pressure, copper atoms diffuse and fuse with each other. Multi-layer copper foils merge into a dense solid monolith at terminals without solder inclusion. After welding, cooling proceeds slowly under pressure instead of immediate pressure relief, releasing residual welding stress to prevent delamination and microcracks caused by cooling rebound. For custom thin sensing flexible connectors

3. Post-welding Processing & Process Sequence
After welding and cooling, flash removal and edge chamfering are carried out on welded areas to eliminate sharp edges. Bending forming is performed afterwards. A safe distance is reserved between bending tangent lines and welding boundaries to avoid stress concentration at the junction of rigid and flexible sections. Tin plating (3~5 μm full coverage) is implemented after forming. Reversed sequence will cause cracking and peeling of tin coating during bending and degrade corrosion resistance. Hole machining is finished after forming to meet tolerance requirements for assembly with standard studs such as M4.
4. Quality Inspection & Acceptance Criteria
Full inspection is performed for every batch. Visual inspection: no pores, cracks or incomplete fusion on welded zones; copper foils in flexible zones slide freely. Electrical test: DC resistance measurement with resistance fluctuation controlled within 3%. Mechanical test: terminal tensile test, fracture shall not occur at welding interface. Elastic rebound test: no permanent deformation after out-of-plane displacement. Thermal cycle and vibration simulation tests are conducted to replicate high-temperature alternating working conditions in UAE and verify anti-delamination performance of welded layers. Material certificates and test reports can be supplied together with shipments to satisfy overseas owner acceptance.
5. Process Control & Project Experience
The core rule of this solution: welding is limited to terminals; no welding reinforcement is permitted on flexible zones. In a previous Middle East transformer project, the customer performed unauthorized spot welding on flexible zones on site. Stress could not be released during operation, resulting in copper foil fracture. Xi'an Zipeng Technology strictly controls welding die boundaries to prevent welding coverage extending into flexible sections. The full diffusion welding process complies with drawing specifications for export projects. Complete welding procedure documents can be provided to ensure long-term stable product operation and reduce after-sales risks for overseas projects.